For machine processing roller transport RT. This is a non-hardening rapid fixer and should not be used with hardener additives. The typical processing temperature is 24 degrees C, but it may be used up to 40 degrees C. Dilution 1:4 with water.

Details

5L concentrate

$74.57
2000RT Developer/Rep - 5ltr
$74.57
Product image 1
Product image 2
Product image 3

Description

For machine processing roller transport RT. This is a non-hardening rapid fixer and should not be used with hardener additives. The typical processing temperature is 24 degrees C, but it may be used up to 40 degrees C. Dilution 1:4 with water.

Details

5L concentrate